Industrial wire woven mesh surface defects

Crease: Partially folded on the mesh surface, forming an irreversible impression.

Holes: There are multiple warps or wefts on the surface of the mesh.

Corrosion: corrosion on the surface of the mesh,

Rust spots: green, brown, or discolored spots appear on the mesh surface.

Broken wire: The meridian or weft thread on the surface of the mesh must be disconnected.

Mosquito mouth: The metal wire makes a circle, twists, and empties the mesh surface.

Top buckle: poor warp joints, top out of the net surface.

Weft reduction: Local cubic meters of weft are bent and the mesh is deformed.

Filament: Two or more wires are woven together in parallel.

Jumping wire (jump shuttle): warp or weft cross stitching error.

Loose wire: Loose displacement of individual warp or weft.

Miscellaneous materials weave in: foreign material weaves in the net.

Cloud weaving: Overlapping wefts or soft and hard inhomogeneities create irregular cloud-like patterns.

Drum kits: The network surface bulges out.

Double line: Warp or weft overlap.

Size hole: uneven mesh mesh size.

Sparse files: The individual meshes of the mesh are suddenly or too small.

Loose edge: The web is wavy and bulging.


Source: China Metal Products Network

High Temperature Filter

High Temperature Filter,Synthetic Fiber No Partition,Hepa High Efficiency Filter,High Temperature Filter Metal Frame

Ningbo Ifilter Purification Equipment CO.,Ltd. , https://www.aifilterparts.com